Angarsk, Irkutsk region, Russian Federation
The effect of the addition of 1-methyl-1-telluracyclohexane iodide to the standard Watts electrolyte was studied using the Hull cell. It is shown that at a current density of 4 A/dm2, a temperature of 50 0C, a pH of 5.4, and a concentration of 0.2 g/l of the additive, a shiny nickel coating is formed.
nickel plating, gloss-forming agents, organotelluric compounds
1. Mamaev V.I., Kudryavcev V.N. Nikelirovanie. M.: Izd. RHTU im. D.I. Mendeleeva. 2014. 192 s.
2. Berezina S.I., Keshner T.D., Hodyrev Yu.P., Voycehovskaya R.N., Al'fonsov V.A. Elektroosazhdenie tverdyh nikelevyh pokrytiy s nizkoy poristost'yu // Zaschita metallov. 1986. T.22. № 1. S.93-95.
3. Bigelis V.M., Karputa O.Ya., Navalihin L.V. Issledovanie vklyucheniy sery i kisloroda v gal'vanicheskih nikelevyh pokrytiyah // Elektrohimiya. 1994. T.30. № 1. S. 107-109